Answer:
The minimum thickness depends on the application. Typical thickness of the concentrator pole on the surface hardening coils is 0.125-0.5″ (3-13mm). In some cases, concentrator thickness as small as 0.020″ (0.5mm) have been used in low power, high frequency applications.
Have more questions? Here are some other related frequently asked questions.
The minimum thickness depends on the application. Typical thickness of the concentrator pole on the surface hardening coils is 0.125-0.5″ (3-13mm). In some cases, concentrator thickness as small as 0.020″ (0.5mm) have been used in low power, high frequency applications.
Have more questions? Here are some other related frequently asked questions.
Have more questions? Here are some other related frequently asked questions.